ASTM A463 Grade SS80 [550]

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Tensile strength Rm

570 MPa at 20 °C

Yield strength YS

550 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

98.79 - 100 %

Ni

0 - 0.2 %

V

0 - 8E-3 %

C

0 - 0.2 %

Ti

0 - 0.03 %