Customize your search with filters
Do you have any questions?
Hardness, Brinell HB
217 [-] at 20 °C
Reduction of area Z
45 % at 20 °C
Tensile strength Rm
415 MPa at 20 °C
Yield strength YS
310 MPa at 20 °C
Element
Weight %
Comment
74.87 - 80.75 %
17.5 - 19.5 %
1.75 - 2.5 %
0 - 0.03 %
0 - 1 %
Processing history
annealed
This material data has been provided by MetalInfo.