Search for materials or suppliers
matmatch.com/materials/MINFM66602

ASTM A312 Grade TP304L

Get more information
Contact Matmatch

Equivalent standards

GB/T 1220 Grade 00Cr19Ni10 GB/T 2100 Grade ZG00Cr18Ni10 GB/T 3280 Grade 00Cr19Ni10 GB/T 4237 Grade 00Cr19Ni10 More GB/T 4240 Grade 00Cr19Ni11-R GB/T 14975 Grade 00Cr19Ni10 GB/T 14976 Grade 00Cr19Ni10 GB 4239 Grade 00Cr19Ni10 GB 4356 Grade 00Cr19Ni11 GB 12770 Grade 00Cr19Ni11 GB 12771 Grade 00Cr19Ni11 GB 13296 Grade 00Cr19Ni10 GOST 5632 Grade 03Kh18N11 GOST 7350 Grade 03Kh18N11 GOST 5582 Grade 03Kh18N11 GOST 5949 Grade 03Kh18N11 GOST 25054 Grade 03Kh18N11 AS 1449 Grade 304LL AS 1444 Grade 304L AS 1449 Grade 304L AS 2837 Grade 304L BDS 6738 Grade 000Ch18N11 BDS 6738 Grade OOCH18N11 CSA G110.9 Grade 304L CSA G110.3 Grade 304L CSA G110.6 Grade 304L CSN 417249 Grade 17249 DIN 17440 Grade X2CrNi1911 DIN 17441 Grade X2CrNi1911 DIN 17455 Grade X2CrNi1911 DIN 17456 Grade X2CrNi1911 DIN 17457 Grade X2CrNi1911 DIN 17458 Grade X2CrNi1911 DIN 2528 Grade X2CrNi1911 DIN 1654-5 Grade X2CrNi1911 SEW 410 Grade G-X2CrNiN189 EN 10028-7 Grade X2CrNi19-11 EURONORM 119-5 Grade X2CrNiN1810KD EURONORM 119-5 Grade X3CrNi1810KD EURONORM 119-5 Grade X2CrNi1810KD EURONORM 88-1 Grade X2CrNi1810 EURONORM 88-2 Grade X2CrNi1810 EURONORM 88-3 Grade X2CrNi1810 EURONORM 119 Grade X3CrNi1810KD EURONORM 141 Grade X3CrNi1810KT SFS 720 SFS 720 Grade X2CrNi1810 NF A32-055 Grade Z2CN18-10M NF A32-056 Grade Z2CN18-10M NF A35-575 Grade Z2CN18-09 NF A35-573 Grade Z2CN18-10 NF A35-575 Grade Z2CN18-10 NF Grade Z2CN18-10M NF Grade Z3CN19-10M NF Grade Z3CN19-9M NF A32-056 Grade Z3CND20-10M NF A32-056 Grade Z2CND18-12M NF A35-572 Grade Z2CN18-10 NF A35-559 Grade Z2CN18-10 NF A35-573 Grade Z1CN18-12 NF A35-573 Grade Z3CN18-10 NF A35-574 Grade Z3CN19-11 NF A35-577 Grade Z3CN19-11FF NF A36-209 Grade Z1CN18-12 NF A36-209 Grade Z3CN18-10 NF A36-607 Grade Z2CN18-10 BS Grade 970-4 BS Grade 1501-3 BS Grade S.536 BS Grade T.74 BS Grade 1502 BS Grade 1503 BS Grade 1504 BS Grade 3100 BS Grade 3606 BS Grade 970-1 BS Grade 6323-8 BS Grade 1449-2 MSZ 4360 Grade KO41LC IS 6528 Grade 02Cr18Ni11 IS 6529 Grade 02Cr18Ni11 IS 6603 Grade 02Cr18Ni11 IS 6911 Grade 02Cr18Ni11 IS 6527 Grade 02Cr18Ni11 COMECON PC4-70 Grade 16 ISO 4954 Grade X2CrNi1810E ISO 2604-1 Grade F46~ ISO 2604-4 Grade X2CrNi1810 ISO 2604-5 Grade TW46~ UNI 3161 Grade GX2CrNi1910 UNI 6901 Grade X2CrNi1811 UNI 6904 Grade X2CrNi1811 UNI 7500 Grade X2CrNi1811 UNI 8317 Grade X2CrNi1811 UNI 6939 Grade X3CrNi1811 UNI 7660 Grade X2CrNi1811KG UNI 7660 Grade X2CrNi1811KW NOM B-229 Grade TP304L NS 14360 NS 14001 Grade 14360 ÖNORM M3120 Grade X2CrNi1911S ÖNORM M3121 Grade X2CrNi1911KKW EN 10088-1 Grade X2CrNi19-11 EN 10088-2 Grade X2CrNi19-11 EN 10088-3 Grade X2CrNi19-11 EN 10216-5 Grade X2CrNi19-11 EN 10217-7 Grade X2CrNi19-11 EN 10272 Grade X2CrNi19-11 COPANT Grade 513 PN 86020 Grade OOH18N10 STAS 3583 Grade 2NiCr185 UNE 36257 Grade AM-X2CrNiMo1911 UNE 36257 Grade AM-X2CrNi1910 UNE 36016-1 Grade X2CrNi1910 UNE 36087 Grade X2CrNi1910 UNE 36016-1 Grade X2CrNi1810 UNE 36016-2 Grade X2CrNi1810 UNE 36087 Grade X2CrNi1810 UNE Grade F.310.G SIS 142352 Grade 2352 AMS 5511 AMS 5647 ASME SA182 Grade 304L ASME SA213 Grade 304L ASME SA240 Grade 304L ASME SA249 Grade 304L ASME SA312 Grade 304L ASME SA403 Grade 304L ASME SA479 Grade 304L ASME SA688 Grade 304L ASTM A213 Grade TP304L ASTM A269 Grade TP304L ASTM A276 Grade 304L ASTM A351 Grade CF3 ASTM A351 Grade CF3A ASTM A403 Grade CR304L ASTM A403 Grade WP304L ASTM A943 Grade TP304L ASTM A959 Grade 304L ASTM A988 Grade 18Cr ASTM A965 Grade F304L ASTM A793 Grade 304L ASTM A182 Grade F304L ASTM A249 Grade TP304L ASTM A270 Grade TP304L ASTM A409 Grade TP304L ASTM A451 Grade CPF3 ASTM A451 Grade CPF3A ASTM A511 Grade MT304L ASTM A554 Grade MT304L ASTM A632 Grade TP304L ASTM A688 Grade TP304L ASTM A774 Grade TP304L ASTM A778 Grade TP304L ASTM A813 Grade TP304L ASTM A814 Grade TP304L ASTM A851 Grade TP304L ASTM A743 Grade CF3 ASTM A744 Grade CF3 ASTM A167 Grade 304L ASTM A240 Grade 304L ASTM A478 Grade 304L ASTM A493 Grade 304L ASTM A580 Grade 304L ASTM A666 Grade 304L ASTM A314 Grade 304L ASTM A336 Grade F304L ASTM A473 Grade 304L ASTM A479 Grade 304L FEDERAL QQ-S-766C Grade 304L FEDERAL QQ-S-763 Grade 304L FEDERAL QQ-S-766 Grade 304L MIL T-8973 Grade 304L MIL P-1144 Grade 304L MIL S-23195 Grade 304L MIL S-23196 Grade 304L MIL S-27419 Grade 304L MIL S-4043 Grade 304L MIL S-862B Grade 304L MIL T-8606 Grade 304L UNS Grade J92500 UNS Grade S30403 STN 417249 Grade 17249 JIS G3463 Grade SUS304LTB JIS G3447 Grade SUS304LTBS JIS G3459 Grade SUS304LTP JIS G4306 Grade SUS304L JIS G4307 Grade SUS304L JIS G3214 Grade SUSF304L JIS G4303 Grade SUS304L JIS G4304 Grade SUS304L JIS G4305 Grade SUS304L JIS G4308 Grade SUS304L JIS G4309 Grade SUS304L JIS G4318 Grade SUS304L JIS G5121 Grade SCS16A JIS G5121 Grade SCS19 JIS G5121 Grade SCS19A AISI 304L ISO 9328-5 Grade X2CrNi1810 ISO TR Grade 15510 EN 10250-4 Grade X2CrNi19-11 SAE J405 Grade 304L ASTM A312 Grade TP304L
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 65.8899 — 73.9999
Cr 18.0 — 20.0
Ni 8.0 — 11.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
P 0.0 — 0.045
C 0.0 — 0.035
S 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

485.00 MPa

Yield strength [ YS ]

170.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66602 to find materials similar to ASTM A312 Grade TP304L.