ASTM A312 Grade TP348

Get more information
Contact Matmatch

Equivalent standards

GB 4239 Grade 0Cr18Ni11Nb GB 12770 Grade 0Cr18Ni11Nb GB 12771 Grade 0Cr18Ni11Nb GB 13296 Grade 0Cr18Ni11Nb More GB 13296 Grade 1Cr19Ni11Nb GB 4356 Grade 0Cr18Ni11Nb GB 2270 Grade 1Cr18ni11Nb GOST 5632 Grade 08Kh18N12B GOST 7350 Grade 08Kh18N12B GOST 5582 Grade 08Kh18N12B GOST 5949 Grade 08Kh18N12B BDS 6738 Grade 0Ch18N12B CSA G110.3 Grade 348 CSA G110.6 Grade 348 CSA G110.9 Grade 348 EURONORM 119-5 Grade XNiCr1816KD EURONORM 88-1 Grade X6CrNiNb1810 EURONORM 88-2 Grade X6CrNiNb1810 EURONORM 88-3 Grade X6CrNiNb1810 EURONORM 95 Grade X10CrNiNb1810 NF A35-572 Grade Z6CNNb18-10 NF A35-573 Grade Z6CNNb18-10 NF A35-574 Grade Z6CNNb18-10 NF A36-209 Grade Z6CNNb18-10 NF A36-607 Grade Z6CNNb18-10 BS Grade 1501-3 BS Grade 2S.130 BS Grade 2S.143 BS Grade 2S.144 BS Grade 2S.145 BS Grade S.525 BS Grade S.527 BS Grade 1502 BS Grade 1503 BS Grade 3606 BS Grade 970-1 BS Grade 1506 BS Grade 1449-2 ISO 2604-1 Grade F50 ISO 2604-1 Grade F52 ISO 2604-2 Grade P50 ISO 2604-4 Grade X6CrNiNb1810 ISO 2604-5 Grade TW50 UNI 6901 Grade X6CrNiNb1811 UNI 6904 Grade X6CrNiNb1811 UNI 7500 Grade X6CrNiNb1811 UNI 7660 Grade X6CrNiNb1811KT UNI 8317 Grade X6CrNiNb1811 UNI 6901 Grade X8CrNiNb1811 UNI 6904 Grade X8CrNiNb1811 UNI 6941 Grade X6CrNiNb1811 UNI 7660 Grade X6CrNiNb1811KG UNI 7660 Grade X6CrNiNb1811KW UNI 8317 Grade X8CrNiNb1811 UNI 8366 Grade G-X6CrNiNb1811 NOM B-83 Grade 348 NOM B-185 Grade TP348 NOM B-229 Grade TP348 NOM B-194 Grade TP348 NOM B-186 Grade TP348 NOM B-218 Grade TP348 ÖNORM M3120 Grade X6CrNiNb1810S ÖNORM M3121 Grade X6CrNiNb1810KKW COPANT Grade 513 PN 86020 Grade OH18N12Nb UNE 36016-1 Grade X6CrNiNb1810 UNE 36016-2 Grade X6CrNiNb1810 UNE 36087 Grade X6CrNiNb1810 ASME SA182 Grade 348 ASME SA213 Grade 348 ASME SA240 Grade 348 ASME SA249 Grade 348 ASME SA312 Grade 348 ASME SA358 Grade 348 ASME SA376 Grade 348 ASME SA403 Grade 348 ASME SA409 Grade 348 ASME SA479 Grade 348 ASTM A213 Grade TP348 ASTM A269 Grade TP348 ASTM A276 Grade 348 ASTM A403 Grade CR348 ASTM A403 Grade WP348 ASTM A943 Grade TP348 ASTM A959 Grade 348 ASTM A965 Grade F348 ASTM A182 Grade F348 ASTM A249 Grade TP348 ASTM A376 Grade TP348 ASTM A409 Grade TP348 ASTM A632 Grade TP348 ASTM A813 Grade TP348 ASTM A814 Grade TP348 ASTM A167 Grade 348 ASTM A240 Grade 348 ASTM A314 Grade 348 ASTM A336 Grade F348 ASTM A473 Grade 348 ASTM A479 Grade 348 ASTM A580 Grade 348 FEDERAL QQ-S-766C Grade 348 FEDERAL QQ-S-766 Grade 348 MIL S-81591 Grade 347 MIL S-23195 Grade 348 MIL S-23196 Grade 348 UNS Grade J92640 UNS Grade S34800 JIS G4307 Grade SUS347 JIS G4303 Grade SUS347 JIS G4304 Grade SUS347 JIS G4308 Grade SUS347 JIS G4309 Grade SUS347 JIS G4318 Grade SUS347 AISI 348 SAE J405 Grade 348 GB 5310 Grade 1Cr19Ni11Nb GB/T 1220 Grade 0Cr18Ni11Nb GB/T 1221 Grade 0Cr18Ni11Nb GB/T 3280 Grade 0Cr18Ni11Nb GB/T 4237 Grade 0Cr18Ni11Nb GB/T 4238 Grade 0Cr18Ni11Nb GB/T 4240 Grade 0Cr18Ni11Nb-Q GB/T 14975 Grade 0Cr18Ni11Nb GB/T 14976 Grade 0Cr18Ni11Nb GB/T 4240 Grade 0Cr18Ni11Nb-R GB 9948 Grade 1Cr19Ni11Nb BDS 6738 Grade OCh18N12B CSA G110.3 Grade 347 CSA G110.6 Grade 347 CSA G110.9 Grade 347 DIN 17440 Grade X6CrNiNb1810 DIN 17441 Grade X6CrNiNb1810 DIN 17455 Grade X6CrNiNb1810 DIN 17456 Grade X6CrNiNb1810 DIN 17457 Grade X6CrNiNb1810 DIN 17458 Grade X6CrNiNb1810 EN 10028-7 Grade X6CrNiNb18-10 BS Grade 970-4 BS BS Grade 3059-2 IS 6529 Grade 04Cr18Ni10Nb40 IS 6911 Grade 04Cr18Ni10Nb40 IS 6529 Grade O4Cr18Ni10Nb40 IS 6911 Grade O4Cr18Ni10Nb40 COMECON PC4-70 Grade 20 NOM B-171 Grade MT347 NOM B-196 Grade TP347 NOM B-218 Grade TP347 NOM B-229 Grade TP347 NOM B-194 Grade TP347 NOM B-150 Grade AE-347 NOM B-185 Grade TP347 NOM B-186 Grade TP347 EN 10088-1 Grade X6CrNiNb18-10 EN 10088-2 Grade X6CrNiNb18-10 EN 10088-3 Grade X6CrNiNb18-10 EN 10216-5 Grade X6CrNiNb18-10 EN 10217-7 Grade X6CrNiNb18-10 EN 10222-5 Grade X6CrNiNb18-10 EN 10272 Grade X6CrNiNb18-10 COPANT Grade R195 UNE 36016-1 Grade X6CrNiNb1811 UNE 36087 Grade X7CrNiNb1811 SIS 142338 Grade 2338-02 SIS 142338 Grade 2338-22 SIS 142338 Grade 2338-23 SIS 142338 Grade 2338-24 SIS 142338 Grade 2338-25 SIS 142338 Grade 2338-26 SIS 142338 Grade 2338-27 SIS 142338 Grade 2338-29 SIS 142338 Grade 2338 AMS 5512 Grade 347 AMS 5556 AMS 5571 AMS 5575 AMS 5654 AMS 5674 AMS 7229 AMS 7490 ASME SA182 Grade 347 ASME SA193 Grade 347 ASME SA194 Grade 347 ASME SA213 Grade 347 ASME SA240 Grade 347 ASME SA249 Grade 347 ASME SA312 Grade 347 ASME SA320 Grade 347 ASME SA358 Grade 347 ASME SA376 Grade 347 ASME SA403 Grade 347 ASME SA409 Grade 347 ASME SA430 Grade 347 ASME SA479 Grade 347 ASTM A213 Grade TP347 ASTM A269 Grade TP347 ASTM A276 Grade 347 ASTM A312 Grade TP347 ASTM A312 Grade TP348 ASTM A320 Grade B8C ASTM A320 Grade B8CA ASTM A403 Grade CR347 ASTM A403 Grade WP347 ASTM A182 Grade F347 ASTM A194 Grade 8C ASTM A249 Grade TP347 ASTM A271 Grade TP347 ASTM A376 Grade TP347 ASTM A409 Grade TP347 ASTM A430 Grade FP347 ASTM A511 Grade MT347 ASTM A554 Grade MT347 ASTM A632 Grade TP347 ASTM A774 Grade TP347 ASTM A778 Grade TP347 ASTM A813 Grade TP347 ASTM A814 Grade TP347 ASTM A193 Grade B8C ASTM A167 Grade 347 ASTM A240 Grade 347 ASTM A313 Grade 347 ASTM A580 Grade 347 ASTM A314 Grade 347 ASTM A336 Grade F347 ASTM A473 Grade 347 ASTM A479 Grade 347 ASTM A193 Grade B8CA ASTM A194 Grade 8CA FEDERAL QQ-S-766C Grade 347 FEDERAL QQ-S-763 Grade 347 FEDERAL QQ-S-766 Grade 347 MIL S-27419 Grade 347 MIL S-862B Grade 347 MIL T-6737B Grade 347 MIL T-8606C Grade 347 MIL T-8808A Grade 347 MIL T-8973 Grade 347 MIL T-16286E Grade CTP-347 MIL P-1144 Grade 347 MIL S-23195 Grade 347 MIL S-23196 Grade 347 UNS Grade S34700 JIS G3463 Grade SUS347TB JIS G3446 Grade SUS347TKA JIS G3459 Grade SUS347TP JIS G4306 Grade SUS347 JIS G3214 Grade SUSF347 JIS G4305 Grade SUS347 AISI 347 ISO 9328-5 Grade X6CrNiNb1810 ISO 9328-5 Grade X7CrNiNb1810 ISO 9330-6 Grade X6CrNiNb1810 ISO TR Grade 15510 ISO 9329-4 Grade X6CrNiNb1811 ISO 9329-4 Grade X7CrNiNb1811 EN 10250-4 Grade X6CrNiNb18-10
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 62.7499 — 73.9999
Cr 17.0 — 20.0
Ni 9.0 — 13.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
Ta 0.0 — 0.1
C 0.0 — 0.08
P 0.0 — 0.04
S 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

515.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A312 Grade TP348:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66629 to find materials similar to ASTM A312 Grade TP348.