Chemical composition

Element Weight %
Fe 67.2399 — 74.9999
Cr 17.0 — 19.0
Ni 8.0 — 10.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
Se 0.0 — 0.35
P 0.0 — 0.2
C 0.0 — 0.15
S 0.0 — 0.06

Properties

Mechanical

Hardness, Brinell [ HB ]

192.00 [-]

Hardness, Rockwell B [ HRB ]

90.00 [-]

Reduction of area [ Z ]

50.00 %

Tensile strength [ Rm ]

515.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.

Technological properties

Processing history
carbide solution treated in the finished condition
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Stainless Steel

The following suppliers might provide ASTM A320 Grade B8FA carbide solution treated in the finished condition:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66676 to find materials similar to ASTM A320 Grade B8FA carbide solution treated in the finished condition.