Hardness, Brinell HB

321 [-] at 20 °C

Hardness, Rockwell C HRC

35 [-] at 20 °C

Reduction of area Z

45 % at 20 °C

Tensile strength Rm

620 - 760 MPa at 20 °C

Yield strength YS

345 - 655 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

61.84 - 72 %

Cr

16 - 18 %

Ni

10 - 14 %

Mo

2 - 3 %

S

0 - 0.03 %

More

Technological properties

Processing history

carbide solution treated and strain hardened

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.