Hardness, Brinell HB
192 [-] at 20 °C
Hardness, Rockwell B HRB
90 [-] at 20 °C
Reduction of area Z
50 % at 20 °C
Tensile strength Rm
515 MPa at 20 °C
Yield strength YS
205 MPa at 20 °C
Element
Weight %
Comment
61.84 - 72 %
16 - 18 %
10 - 14 %
2 - 3 %
0 - 0.03 %
Processing history
carbide solution treated in the finished condition
This material data has been provided by MetalInfo.