Chemical composition

Element Weight %
Fe 96.6149 — 97.6799
Mn 0.75 — 1.0
Ni 0.4 — 0.7
Cr 0.4 — 0.6
C 0.38 — 0.43
Si 0.15 — 0.35
Mo 0.2 — 0.3
S 0.0 — 0.04
P 0.0 — 0.005

Properties

Mechanical

Reduction of area [ Z ]

50.00 %

Tensile strength [ Rm ]

860.00 MPa

Yield strength [ YS ]

725.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.

Technological properties

Processing history
quenched and tempered
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A320 Grade L7C quenched and tempered:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66708 to find materials similar to ASTM A320 Grade L7C quenched and tempered.