ASTM A335 Grade P1 pipe (seamless, welded)

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Tensile strength Rm

0 - 380 MPa at 20 °C

Yield strength YS

0 - 205 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

97.8 - 99.15 %

Mo

0.44 - 0.65 %

Mn

0.3 - 0.8 %

C

0.1 - 0.2 %

Si

0.01 - 0.5 %

More

This material data has been provided by MetalInfo.