Chemical composition

Element Weight %
Fe 96.0514 — 97.7099
Cr 1.0 — 1.5
Si 0.5 — 1.0
Mo 0.44 — 0.65
Mn 0.3 — 0.6
C 0.05 — 0.15
P 0.0 — 0.025
S 0.0 — 0.0235

Properties

Mechanical

Tensile strength [ Rm ]

0—415.00 MPa

Yield strength [ YS ]

0—205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66720 to find materials similar to ASTM A335 Grade P11 pipe (seamless, welded).