MIL 6Al-Sn-4Zr-2Mo Annealed or Solution Treated Bar

.XLSX
.PDF
Save

Properties

Mechanical

Elongation A

10 % at 20 °C

Tensile strength Rm

896 MPa at 20 °C

Yield strength YS

827 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Ti

84.18 %

Al

5.5 - 6.5 %

Zr

3.6 - 4.4 %

Sn

1.8 - 2.2 %

Mo

1.8 - 2.2 %

More

Technological properties

Processing history

annealed or solution treated