Chemical composition

Element Weight %
Fe 60.9199 — 66.2099
Cr 24.5 — 26.5
Ni 4.75 — 6.0
Cu 2.75 — 3.25
Mo 1.75 — 2.25
Mn 0.0 — 1.0
P 0.0 — 0.04
C 0.0 — 0.04
Si 0.0 — 0.04

Properties

Mechanical

Tensile strength [ Rm ]

690.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A351 Grade CD4MCu:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66884 to find materials similar to ASTM A351 Grade CD4MCu.