Matmatch helps you find, evaluate and source the best materials for your projects.
Search for materials, projects or suppliers
matmatch.com/materials/MINFM66893

ASTM A351 Grade CF3M

Get more information
Contact Matmatch

Equivalent standards

GB/T 1220 Grade 00Cr17Ni14Mo2 GB/T 4240 Grade 00Cr17Ni14Mo2-Q GB/T 4240 Grade 00Cr17Ni14Mo2-R GB 4239 Grade 00Cr17Ni14Mo2 More GB 4356 Grade 00Cr17Ni14Mo2 GB 12770 Grade 00Cr17Ni14Mo2 GB 12771 Grade 00Cr17Ni14Mo2 GB 13296 Grade 00Cr17Ni14Mo2 GB 2270 Grade 00Cr17Ni14Mo2 AS 1449 Grade 316L AS 2837 Grade 316L BDS 6738 Grade 000Ch17N14M2 CSN 417349 Grade 17349 DIN 17440 Grade X2CrNiMo17132 DIN 17441 Grade X2CrNiMo17132 DIN 17455 Grade X2CrNiMo17132 DIN 17456 Grade X2CrNiMo17132 DIN 17457 Grade X2CrNiMo17132 DIN 17458 Grade X2CrNiMo17132 DIN 2528 Grade X2CrNiMo17132 SEW 410 Grade G-X2CrNiMoN1810 EN 10028-7 Grade X2CrNiMo17-12-2 EURONORM 88-1 Grade X2CrNiMo17132 EURONORM 88-2 Grade X2CrNiMo17132 EURONORM 88-3 Grade X2CrNiMo17132 EURONORM 119 Grade X3CrNiMo17122KD SFS 750 Grade X2CrNiMo17122 NF A32-055 Grade Z2CN18-10M NF A32-056 Grade Z2CN18-10M NF Grade Z2CN18-10M NF Grade Z3CN19-9M NF A32-056 Grade Z3CND20-10M NF A32-056 Grade Z2CND18-12M NF A32-056 Grade Z3CND19-10M NF A32-055 Grade Z2CND18-12M NF A32-056 Grade Z6CND18-12M NF A35-575 Grade Z2CND17-12 NF A36-209 Grade Z2CND17-12 NF A36-607 Grade Z2CND17-12 NF A35-573 Grade Z3CND17-11-02 NF A35-573 Grade Z3CND18-12-03 NF A35-574 Grade Z3CND17-11-02 NF A35-574 Grade Z3CND18-12-02 NF A35-577 Grade Z3CND17-12-02FF NF A36-209 Grade Z3CND17-11-02 NF A36-209 Grade Z3CND18-12-03 NF A36-607 Grade Z2CND18-13 BS Grade 1501-3 BS Grade S.537 BS Grade T.75 BS Grade 1502 BS Grade 1503 BS Grade 1504 BS Grade 2056 BS Grade 3100 BS Grade 3606 BS Grade 970-1 BS Grade 1449-2 ISO 4954 Grade X2CrNiMo17133E ISO 2604-1 Grade F59~ ISO 2604-4 Grade X2CrNiMo1712 ISO 2604-5 Grade TW57 UNI 3161 Grade GX2CrNiMo1911 UNI 6901 Grade X2CrNiMo1712 UNI 6904 Grade X2CrNiMo1712 UNI 7500 Grade X2CrNiMo1712 UNI 8317 Grade X2CrNiMo1712 ÖNORM M3121 Grade X2CrNiMo17132KKW EN 10088-1 Grade X2CrNiMo17-12-2 EN 10088-2 Grade X2CrNiMo17-12-2 EN 10088-3 Grade X2CrNiMo17-12-2 EN 10216-5 Grade X2CrNiMo17-12-2 EN 10217-7 Grade X2CrNiMo17-12-2 EN 10222-5 Grade X2CrNiMo17-12-2 EN 10272 Grade X2CrNiMo17-12-2 EN 10269 Grade X2CrNiMo17-12-2 PN 86020 Grade OOH17N14M2 UNE 36257 Grade AM-X2CrNiMo1911 UNE 36257 Grade AM-X2CrNi1910 UNE 36016-1 Grade X2CrNiMo17123 UNE 36016-1 Grade X2CrNiMo17132 UNE 36016-1 Grade X2CrNiMo17133 UNE 36016-2 Grade X2CrNiMo17132 UNE 36016-2 Grade X2CrNiMo17133 UNE 36087 Grade X2CrNiMo17132 UNE Grade F.310.K SIS 142348 Grade 2348 ANSI A296 Grade CF3 ASTM A351 Grade CF3MA ASTM A351 Grade CF3MN ASTM A451 Grade CPF3M ASTM A744 Grade CF3M UNS Grade J92700 UNS Grade J92800 STN 417349 Grade 17349 JIS G4307 Grade SUS316L JIS G4303 Grade SUS316L JIS G4304 Grade SUS316L JIS G4308 Grade SUS316L JIS G4309 Grade SUS316L JIS G4318 Grade SUS316L ISO 9328-5 Grade X2CrNiMo1712 ISO 4991 Grade C57 ISO 9330-6 Grade X2CrNiMo1712 ISO TR Grade 15510 ISO 9329-4 Grade X2CrNiMo1712 EN 10250-4 Grade X2CrNiMo17-12-2 ASTM A351 Grade CF3M
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 61.0699 — 70.9599
Cr 18.0 — 21.0
Ni 9.0 — 13.0
Mo 2.0 — 3.0
Mn 0.0 — 1.5
Si 0.0 — 0.4
P 0.0 — 0.04
C 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

485.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A351 Grade CF3M:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66893 to find materials similar to ASTM A351 Grade CF3M.