Chemical composition

Element Weight %
Fe 56.5199 — 65.9599
Cr 22.0 — 26.0
Ni 12.0 — 15.0
Mn 0.0 — 1.5
Mo 0.0 — 0.5
Si 0.0 — 0.4
C 0.0 — 0.08
P 0.0 — 0.04

Properties

Mechanical

Tensile strength [ Rm ]

450.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

There are no similar materials at this moment.
Go to matmatch.com/materials/MINFM66905 to find materials similar to ASTM A351 Grade CH8.