ASTM A352 Grade LCA

Get more information
Contact Matmatch

Equivalent standards

Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 95.3349 — 99.9999
Mn 0.0 — 0.7
Si 0.0 — 0.6
Cr 0.0 — 0.5
Ni 0.0 — 0.5
Cu 0.0 — 0.3
C 0.0 — 0.25
Mo 0.0 — 0.2
S 0.0 — 0.045
P 0.0 — 0.04
V 0.0 — 0.03
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software