ASTM A352 Grade LC4

Get more information
Contact Matmatch

Equivalent standards

Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 93.3649 — 95.4999
Ni 4.0 — 5.0
Mn 0.5 — 0.8
Si 0.0 — 0.6
C 0.0 — 0.15
S 0.0 — 0.045
P 0.0 — 0.04
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A352 Grade LC4:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM66921 to find materials similar to ASTM A352 Grade LC4.