Chemical composition

Element Weight %
Fe 87.4049 — 91.4999
Ni 8.5 — 10.0
Mn 0.0 — 0.9
Cr 0.0 — 0.5
Si 0.0 — 0.45
Cu 0.0 — 0.3
Mo 0.0 — 0.2
C 0.0 — 0.13
S 0.0 — 0.045
P 0.0 — 0.04
V 0.0 — 0.03