Elongation A50 A50
0 - 12 % at 20 °C
Tensile strength Rm
0 - 550 MPa at 20 °C
Yield strength YS
0 - 480 MPa at 20 °C
Element
Weight %
Comment
0 - 0.2 %
0 - 0.15 %
0 - 0.2 %
0 - 1.65 %
0 - 0.16 %
This material data has been provided by ASTM.