General

Density ρ

7.6 - 7.7 g/cm³ at 20 °C

Typical for Martensitic Stainless Steel

Mechanical

Elongation A50 A50

0 - 18 % at 20 °C

Hardness, Brinell HB

167 - 229 [-] at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Typical for Martensitic Stainless Steel

Reduction of area Z

0 - 35 % at 20 °C

Tensile strength Rm

0 - 585 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

0 - 380 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1E-5 - 1.3E-5 1/K at 20 °C

Typical for Martensitic Stainless Steel

Melting point Tm

1375 - 1450 °C

Typical for Martensitic Stainless Steel

Thermal conductivity λ

22 - 24 W/(m·K) at 20 °C

Typical for Martensitic Stainless Steel

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.