ASTM A182 Grade F316L Solution-Annealed

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

7.9 - 8.2 g/cm³ at 20 °C

Typical for Austenitic Stainless Steel

Mechanical

Elastic modulus E

195 GPa at 20 °C

Typical for Austenitic Stainless Steel

Elongation A50 A50

30 % at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Typical for Austenitic Stainless Steel

Reduction of area Z

50 % at 20 °C

Tensile strength Rm

485 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

170 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.7E-5 - 1.9E-5 1/K at 20 °C

Typical for Austenitic Stainless Steel

Melting point Tm

1375 - 1450 °C

Typical for Austenitic Stainless Steel

Specific heat capacity cp

440 J/(kg·K) at 20 °C

Typical for Austenitic Stainless Steel

Thermal conductivity λ

11 - 21 W/(m·K) at 20 °C

Typical for Austenitic Stainless Steel

Electrical

Electrical resistivity ρel

8.5E-7 Ω·m at 20 °C

Typical for Austenitic Stainless Steel

Chemical properties

Element

Weight %

Comment

Cr

16 - 18 %

Ni

10 - 15 %

Mn

2 %

Mo

2 - 3 %

Si

1 %

More

This material data has been provided by ASTM.