Tensile strength Rm
550 MPa at 20 °C
Yield strength YS
240 MPa at 20 °C
Element
Weight %
Comment
62.1 - 71 %
16 - 18 %
11 - 14 %
2 - 3 %
0 - 0.03 %
This material data has been provided by MetalInfo.