ASTM A387 Grade 911

Chemical composition

Element Weight %
Fe 85.409989.1096
Cr 8.510.5
W 0.91.1
Mo 0.91.1
Mn 0.30.6
Si 0.10.5
Ni 0.00.4
C 0.090.13
Nb 0.060.1
N 0.040.09
Al 0.00.04
P 0.00.02
S 0.00.01
B 0.03.0E-4

Properties

Mechanical
Tensile strength, Rm
0—840.00 MPa
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.