ASTM A403 Grade CRS31725

Get more information
Contact Matmatch

Chemical composition

Element Weight %
Fe 53.7949 — 64.4999
Cr 18.0 — 20.0
Ni 13.5 — 17.5
Mo 4.0 — 5.0
Mn 0.0 — 2.0
Si 0.0 — 0.75
Cu 0.0 — 0.75
N 0.0 — 0.1
P 0.0 — 0.045
C 0.0 — 0.03
S 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

515.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Stainless Steel

The following suppliers might provide ASTM A403 Grade CRS31725:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM68021 to find materials similar to ASTM A403 Grade CRS31725.