Chemical composition

Element Weight %
Fe 37.3599 — 42.3099
Ni 31.0 — 33.0
Cr 26.0 — 28.0
Mn 0.0 — 1.0
Nb 0.1 — 0.6
Si 0.0 — 0.3
Ce 0.05 — 0.1
C 0.04 — 0.08
Al 0.0 — 0.025
P 0.0 — 0.02
S 0.0 — 0.015

Properties

Mechanical

Tensile strength [ Rm ]

500.00 MPa

Yield strength [ YS ]

185.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Stainless Steel

The following suppliers might provide ASTM A403 Grade CRS33228:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM68022 to find materials similar to ASTM A403 Grade CRS33228.