Customize your search with filters
Do you have any questions?
Tensile strength Rm
690 MPa at 20 °C
Yield strength YS
380 MPa at 20 °C
Element
Weight %
Comment
51.87 - 62.1 %
20.5 - 23.5 %
11.5 - 13.5 %
4 - 6 %
1.5 - 3 %
This material data has been provided by MetalInfo.