Matmatch helps you find, evaluate and source the best materials for your projects.
Search for materials or suppliers
matmatch.com/materials/MINFM68031

ASTM A403 Grade WP316

Get more information
Contact Matmatch

Equivalent standards

GB/T 1220 Grade 0Cr17Ni12Mo2 GB/T 1221 Grade 0Cr17Ni12Mo2 GB/T 3280 Grade 0Cr17Ni12Mo2 GB/T 4237 Grade 0Cr17Ni12Mo2 More GB/T 4238 Grade 0Cr17Ni12Mo2 GB/T 4240 Grade 0Cr17Ni12Mo2-Q GB/T 14975 Grade 0Cr17Ni12Mo2 GB/T 14976 Grade 0Cr17Ni12Mo2 GB/T 4240 Grade 0Cr17Ni12Mo2-L GB/T 4240 Grade 0Cr17Ni12Mo2-R GB 4239 Grade 0Cr17Ni12Mo2 GB 12770 Grade 00Cr17Ni14Mo2 GB 12770 Grade 0Cr17Ni12Mo2 GB 12771 Grade 0Cr17Ni12Mo2 GB 13296 Grade 0Cr17Ni12Mo2 GB 4356 Grade 0Cr17Ni12Mo2 AS 1444 Grade 316 AS 1449 Grade 316 AS 2837 Grade 316 BDS 9631 Grade OCh18N10M2SL CSA G110.3 Grade 316 CSA G110.6 Grade 316 CSA G110.9 Grade 316 CSN 417346 Grade 17346 CSN 417352 Grade 17352 DIN 17224 Grade X5CrNiMo1810 DIN 17440 Grade X5CrNiMo17122 DIN 17440 Grade X5CrNiMo17133 DIN 17441 Grade X5CrNiMo17122 DIN 17441 Grade X5CrNiMo17133 DIN 17455 Grade X5CrNiMo17122 DIN 17455 Grade X5CrNiMo17133 DIN 17456 Grade X5CrNiMo17122 DIN 17456 Grade X5CrNiMo17133 DIN 17457 Grade X5CrNiMo17122 DIN 17457 Grade X5CrNiMo17133 DIN 17458 Grade X5CrNiMo17122 DIN 17458 Grade X5CrNiMo17133 DIN 2528 Grade X5CrNiMo17122 DIN 5512-3 Grade X5CrNiMo17122 DIN 1654-5 Grade X5CrNiMo17122 EN 10028-7 Grade X5CrNiMo17-12-2 EURONORM 119-5 Grade X6CrNiMo1722KD EURONORM 88-1 Grade X5CrNiMo17122 EURONORM 88-1 Grade X5CrNiMo17133 EURONORM 88-2 Grade X5CrNiMo17122 EURONORM 88-2 Grade X5CrNiMo17133 EURONORM 88-3 Grade X5CrNiMo17122 EURONORM 88-3 Grade X5CrNiMo17133 EURONORM 119 Grade X6CrNiMo17122KD SFS 757 Grade X4CrNiMo17123 NF A35-573 Grade Z6CND17-11 NF A35-575 Grade Z6CND17-11 NF A35-572 Grade Z6CNFT17-12 NF A35-572 Grade Z6CND17-11 NF A35-574 Grade Z6CND17-11 NF A35-577 Grade Z6CND17-11 NF A36-209 Grade 6CND17-11 NF A36-607 Grade Z6CND17-11 NF A35-573 Grade Z3CND17-11-01 NF A35-573 Grade Z6CND18-12-03 NF A35-573 Grade Z7CND17-11-02 NF A35-574 Grade Z7CND17-12-02 NF A35-574 Grade Z7CND18-12-03 NF A35-577 Grade Z6CND17-11-02FF NF A36-209 Grade Z6CND18-12-03 NF A36-209 Grade Z7CND17-11-02 BS Grade 970-4 BS BS Grade 1501-3 BS Grade 1502 BS Grade 1503 BS Grade 1554 BS Grade 3059-2 BS Grade 3111-2 BS Grade 3606 BS Grade 970-1 BS Grade 6323-8 BS Grade 1506 BS Grade 1449-2 IS 6527 Grade 04Cr17Ni12M02 IS 6528 Grade 04Cr17Ni12Mo2 IS 6529 Grade 04Cr17Ni12Mo2 IS 6603 Grade 04Cr17Ni12Mo2 IS 6911 Grade 04Cr17Ni12Mo2 IS 6527 Grade O4Cr17Ni12Mo2 IS 6528 Grade O4Cr17Ni12Mo2 IS 6529 Grade O4Cr17Ni12Mo2 IS 6603 Grade O4Cr17Ni12Mo2 IS 6911 Grade O4Cr17Ni12Mo2 ISO 2604-2 Grade TS60 ISO 2604-2 Grade TS61 ISO 2604-4 Grade P60 ISO 2604-4 Grade P61 ISO 4954 Grade X5CrNiMo17122E ISO 6931 Grade X5CrNiMo17122 ISO 2604-1 Grade F62~ ISO 2604-4 Grade X5CrNiMo1712 ISO 2604-5 Grade TW60~ ISO 2604-1 Grade F62 ISO 2604-4 Grade X5CrNiMo1713 ISO 2604-5 Grade TW61~ UNI 6901 Grade X5CrNiMo UNI 6904 Grade X5CrNiMo1712 UNI 8317 Grade X5CrNiMo1712 UNI 6901 Grade X5CrNiMo1712 UNI 6901 Grade X5CrNiMo1713 UNI 6901 Grade X8CrNiMo1713 UNI 6904 Grade X5CrNiMo1713 UNI 6904 Grade X8CrNiMo1713 UNI 7500 Grade X5CrNiMo1712 UNI 7500 Grade X5CrNiMo1713 UNI 7660 Grade X5CrNiMo1712KG UNI 7660 Grade X5CrNiMo1712KW UNI 8317 Grade X5CrNiMo1713 UNI 8366 Grade X5CrNiMo1712 NOM B-186 Grade 1682H NOM B-83 Grade 316 NOM B-186 Grade TP316 NOM B-128 Grade TP316 NOM B-229 Grade TP316 NOM B-150 Grade AE-316 NOM B-185 Grade TP316 NS 14001 Grade 14450 ÖNORM M3120 Grade X5CrNiMo17122S ÖNORM M3121 Grade X5CrNiMo17122KKW ÖNORM M3121 Grade X5CrNiMo17133KW EN 10088-1 Grade X5CrNiMo17-12-2 EN 10088-2 Grade X5CrNiMo17-12-2 EN 10088-3 Grade X5CrNiMo17-12-2 EN 10216-5 Grade X5CrNiMo17-12-2 EN 10217-7 Grade X5CrNiMo17-12-2 EN 10222-5 Grade X5CrNiMo17-12-2 EN 10272 Grade X5CrNiMo17-12-2 EN 10269 Grade X5CrNiMo17-12-2 COPANT Grade 513 UNE 36016-1 Grade XCrNiMo17-12-03 UNE 36016-1 Grade X5CrNiMo17122 UNE 36016-1 Grade X5CrNiMo17133 UNE 36016-2 Grade X5CrNiMo17122 UNE 36016-2 Grade X5CrNiMo17133 UNE 36087 Grade X5CrNiMo17122 UNE 36087 Grade X5CrNiMo17133 UNE Grade F.310.A SIS 142343 Grade 2343-04 SIS 142343 Grade 2343-22 SIS 142343 Grade 2343-23 SIS 142343 Grade 2343-24 SIS 142343 Grade 2343-26 SIS 142343 Grade 2343-27 SIS 142343 Grade 2343-28 SIS 142343 Grade 2343-29 SIS 142347 Grade 2347-02 SIS 142347 Grade 2347-22 SIS 142347 Grade 2347-23 SIS 142347 Grade 2347-24 SIS 142347 Grade 2347-25 SIS 142347 Grade 2347-26 SIS 142347 Grade 2347-27 SIS 142347 Grade 2347-28 SIS 142347 Grade 2347-29 SIS 142343 Grade 2343 SIS 142347 Grade 2347 AMS 5573 AMS 5648 AMS 5690 AMS 5696 ASME SA182 Grade 316 ASME SA193 Grade 316 ASME SA194 Grade 316 ASME SA213 Grade 316 ASME SA240 Grade 316 ASME SA249 Grade 316 ASME SA312 Grade 316 ASME SA320 Grade 316 ASME SA358 Grade 316 ASME SA376 Grade 316 ASME SA403 Grade 316 ASME SA409 Grade 316 ASME SA430 Grade 316 ASME SA479 Grade 316 ASME SA688 Grade 316 ASTM A213 Grade TP316 ASTM A269 Grade TP316 ASTM A276 Grade 316 ASTM A312 Grade TP316 ASTM A320 Grade B8M ASTM A320 Grade B8MA ASTM A403 Grade CR316 ASTM A943 Grade TP316 ASTM A959 Grade 316 ASTM A988 Grade 18Cr ASTM A965 Grade F316 ASTM A793 Grade 316 ASTM A182 Grade F316 ASTM A194 Grade 8M ASTM A249 Grade TP316 ASTM A270 Grade TP316 ASTM A271 Grade TP316 ASTM A376 Grade TP316 ASTM A409 Grade TP316 ASTM A430 Grade FP316 ASTM A511 Grade MT316 ASTM A554 Grade MT316 ASTM A632 Grade TP316 ASTM A688 Grade TP316 ASTM A813 Grade TP316 ASTM A814 Grade TP316 ASTM A826 Grade TP316 ASTM A193 Grade B8M ASTM A167 Grade 316 ASTM A240 Grade 316 ASTM A313 Grade 316 ASTM A368 Grade 316 ASTM A478 Grade 316 ASTM A492 Grade 316 ASTM A493 Grade 316 ASTM A580 Grade 316 ASTM A666 Grade 316 ASTM A314 Grade 316 ASTM A336 Grade F316 ASTM A473 Grade 316 ASTM A479 Grade 316 ASTM A831 Grade 316 ASTM A771 Grade TP316 ASTM A193 Grade B8MA ASTM A193 Grade B8M2 ASTM A193 Grade B8M3 ASTM A194 Grade 8MA FEDERAL QQ-S-766C Grade 316 FEDERAL QQ-S-763 Grade 316 FEDERAL QQ-A-766 Grade 316 MIL P-1144 Grade 316 MIL S-5059 Grade 316 MIL S-7720 Grade 316 MIL S-862B Grade 316 UNS Grade S31600 STN 417346 Grade 17346 STN 417352 Grade 17352 JIS G3463 Grade SUS316TB JIS G3447 Grade SUS316TBS JIS G3446 Grade SUS316TKA JIS G3459 Grade SUS316TP JIS G4306 Grade SUS316 JIS G4307 Grade SUS316 JIS G3214 Grade SUSF316 JIS G4303 Grade SUS316 JIS G4304 Grade SUS316 JIS G4305 Grade SUS316 JIS G4308 Grade SUS316 JIS G4309 Grade SUS316 JIS G4314 Grade SUS316 JIS G4316 Grade SUSY316 JIS G4318 Grade SUS316 AISI 316 ISO 9328-5 Grade X5CrNiMo1712 ISO 6931-1 Grade X5CrNiMo17-12-2 ISO 9330-6 Grade X5CrNiMo1712 ISO TR Grade 15510 ISO 9329-4 Grade X5CrNiMo1712 EN 10250-4 Grade X5CrNiMo17-12-2 EN 10270-3 Grade X5CrNiMo17-12-2 SAE J405 Grade 316 EN 10028-7 Grade X3CrNiMo17-13-3 EN 10088-1 Grade X3CrNiMo17-13-3 EN 10088-2 Grade X3CrNiMo17-13-3 EN 10088-3 Grade X3CrNiMo17-13-3 EN 10216-5 Grade X3CrNiMo17-13-3 EN 10217-7 Grade X3CrNiMo17-13-3 EN 10222-5 Grade X4CrNiMo17-13-3 EN 10272 Grade X3CrNiMo17-13-3 ASTM A403 Grade WP316 EN 10250-4 Grade X3CrNiMo17-13-3
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 61.8449 — 71.9999
Cr 16.0 — 18.0
Ni 10.0 — 14.0
Mo 2.0 — 3.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
C 0.0 — 0.08
P 0.0 — 0.045
S 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

515.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Stainless Steel

The following suppliers might provide ASTM A403 Grade WP316:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM68031 to find materials similar to ASTM A403 Grade WP316.