ASTM A403 Grade WP321

Get more information
Contact Matmatch

Equivalent standards

YB/T 5092 Grade H0Cr20Ni10Ti GB/T 4240 Grade 0Cr18Ni11Ti-Q GB/T 1220 Grade 0Cr18Ni10Ti GB/T 1221 Grade 0Cr18Ni10Ti More GB/T 3280 Grade 0Cr18Ni10Ti GB/T 4237 Grade 0Cr18Ni10Ti GB/T 4238 Grade 0Cr18Ni10Ti GB/T 4240 Grade 0Cr18Ni11Ti-R GB/T 14975 Grade 0Cr18Ni10Ti GB/T 14976 Grade 0Cr18Ni10Ti GB 4242 Grade H0Cr20Ni10Ti GB 12771 Grade 0Cr18Ni11Ti GB 13296 Grade 0Cr18Ni10Ti GB 13296 Grade 1Cr18Ni11Ti GB 4356 Grade 0Cr18Ni11Ti GB 2270 Grade 0Cr18Ni9Ti GOST 5632 Grade 08Kh18N10T GOST 5632 Grade 12Kh18N10T GOST 7350 Grade 08Kh18N10T GOST 7350 Grade 12Kh18N10T GOST 4986 Grade 08Kh18N10T GOST 4986 Grade 12Kh18N10T GOST 5582 Grade 08Kh18N10T GOST 5582 Grade 12Kh18N10T GOST 5949 Grade 08Kh18N10T GOST 5949 Grade 12Kh18N10T GOST 18907 Grade 08Kh18N10T GOST 18907 Grade 12Kh18N10T GOST 25054 Grade 08Kh18N10T GOST 25054 Grade 12Kh18N10T GOST 10498 Grade 06Ch18N10T GOST 24030 Grade 08Ch18N10T GOST 10498 Grade 09Ch18N10T AS 2837 Grade 321 AS 1449 Grade 321 BDS 6738 Grade Ch18N9T BDS 6738 Grade 0Ch18N10T CSA G110.3 Grade 321 CSA G110.6 Grade 321 CSA G110.9 Grade 321 CSN 417246 Grade 17246 CSN 417247 Grade 17247 CSN 417248 Grade 17248 DIN 1654-5 Grade X6CrNiTi1810 DIN 17440 Grade X6CrNiTi1810 DIN 17441 Grade X6CrNiTi1810 DIN 17455 Grade X6CrNiTi1810 DIN 17456 Grade X6CrNiTi1810 DIN 17457 Grade X6CrNiTi1810 DIN 17458 Grade X6CrNiTi1810 DIN 2528 Grade X6CrNiTi1810 DIN 4133 Grade X6CrNiTi1810 DIN 43720 Grade X6CrNiTi1810 DIN 5512-3 Grade X6CrNiTi1810 DIN 1654-5 Grade X6CrNiMoTi17122 EN 10028-7 Grade X6CrNiTi18-10 EURONORM 88-1 Grade X6CrNiTi1810 EURONORM 88-2 Grade X6CrNiTi1810 EURONORM 88-3 Grade X6CrNiTi1810 EURONORM 95 Grade X10CrNiTi1810 EURONORM 141 Grade X6CrNiTi1810KT NF A35-572 Grade Z6CNT18-10 NF A35-574 Grade Z6CNT18-10 NF A35-573 Grade Z6CNT18-10 NF A36-209 Grade Z6CNT18-10 NF A36-607 Grade Z6CNT18-10 BS Grade 970-4 BS Grade A8.Ti BS Grade 1501-3 BS Grade 1502 BS Grade 1503 BS Grade 3606 BS Grade 1506 BS Grade 6323-8 MSZ 4360 Grade KO36Ti MSZ 4360 Grade KO37Ti IS 6529 Grade 04Cr17Ni12Mo2Ti20 IS 6603 Grade 04Cr17Ni12Mo2Ti20 IS 6911 Grade 04Cr17Ni12Mo2Ti20 IS 6529 Grade 04Cr18Ni10Ti20 IS 6603 Grade 04Cr18Ni10Ti20 IS 6911 Grade 04Cr18Ni10Ti20 ISO 2604-1 Grade F53 ISO 2604-1 Grade F55 ISO 2604-2 Grade TS53 ISO 2604-4 Grade X6CrNiTi1810 ISO 2604-5 Grade TW53 UNI 6901 Grade X6CrNiTi1811 UNI 6904 Grade X6CrNiTi1811 UNI 7500 Grade X6CrNiTi1811 UNI 7660 Grade X6CrNiTi1811KG UNI 7660 Grade X6CrNiTi1811KW UNI 7660 Grade X6CrNiTi1811KT UNI 8317 Grade X6CrNiTi1811 NOM B-83 Grade 321 NOM B-171 Grade MT321 NOM B-185 Grade TP321 NOM B-196 Grade TP321 NOM B-218 Grade TP321 NOM B-229 Grade TP321 NOM B-194 Grade TP321 NS 14001 Grade 14355 ÖNORM M3120 Grade X6CrNiTi1810S ÖNORM M3121 Grade X6CrNiTi1810KKW EN 10088-1 Grade X6CrNiTi18-10 EN 10088-2 Grade X6CrNiTi18-10 EN 10088-3 Grade X6CrNiTi18-10 EN 10216-5 Grade X6CrNiTi18-10 EN 10217-7 Grade X6CrNiTi18-10 EN 10222-5 Grade X6CrNiTi18-10 EN 10272 Grade X6CrNiTi18-10 COPANT Grade 513 COPANT Grade R195 PN 86020 Grade OH18N10T PN 86020 Grade 1H18N9T STAS 3583 Grade 10TiNiCr180 UNE 36016-1 Grade X6CrNiTi1810 UNE 36016-2 Grade X6CrNiTi1810 UNE 36087 Grade X6CrNiTi1810 UNE Grade F.332 SIS 142337 Grade 2337-22 SIS 142337 Grade 2337-23 SIS 142337 Grade 2337-24 SIS 142337 Grade 2337-25 SIS 142337 Grade 2337-26 SIS 142337 Grade 2337-28 SIS 142337 Grade 2337-29 SIS 142337 Grade 2337 AMS 5510 Grade 321 ASTM A213 Grade TP321 ASTM A269 Grade TP321 ASTM A276 Grade 321 ASTM A312 Grade TP321 ASTM A320 Grade B8T ASTM A320 Grade B8TA ASTM A403 Grade CR321 ASTM A943 Grade TP321 ASTM A959 Grade 321 ASTM A965 Grade F321 ASTM A182 Grade F321 ASTM A194 Grade 8T ASTM A249 Grade TP321 ASTM A271 Grade TP321 ASTM A376 Grade TP321 ASTM A409 Grade TP321 ASTM A430 Grade FP321 ASTM A511 Grade MT321 ASTM A554 Grade MT321 ASTM A632 Grade TP321 ASTM A774 Grade TP321 ASTM A778 Grade TP321 ASTM A813 Grade TP321 ASTM A814 Grade TP321 ASTM A193 Grade B8T ASTM A167 Grade 321 ASTM A240 Grade 321 ASTM A313 Grade 321 ASTM A580 Grade 321 ASTM A314 Grade 321 ASTM A336 Grade F321 ASTM A473 Grade 321 ASTM A479 Grade 321 ASTM A193 Grade B8TA ASTM A194 Grade 8TA FEDERAL QQ-S-766C Grade 321 MIL P-1144 Grade 321 MIL S-27419 Grade 321 MIL S-862B Grade 321 MIL T-6737B Grade 321 MIL T-8606C Grade 321 MIL T-8808A Grade 321 MIL T-8973 Grade 321 MIL T-16286E Grade CTP-321 UNS Grade S32100 STN 417246 Grade 17246 STN 417247 Grade 17247 STN 417248 Grade 17248 JIS G3463 Grade SUS321TB JIS G3446 Grade SUS321TKA JIS G3459 Grade SUS321TP JIS G4306 Grade SUS321 JIS G3214 Grade SUSF321 JIS G4303 Grade SUS321 JIS G4308 Grade SUS321 JIS G4316 Grade SUSY321 AISI 321 BS Grade 1449-2 ISO 9328-5 Grade X6CrNiTi1810 ISO 9330-6 Grade X6CrNiTi1810 ISO TR Grade 15510 ISO 4954 Grade X6CrNiTi1810E ISO 9329-4 Grade X6CrNiTi1810 EN 10250-4 Grade X6CrNiTi18-10 SAE J405 Grade 321 GB/T 1220 Grade 1Cr18Ni9Ti GB/T 1221 Grade 1Cr18Ni9Ti GB/T 3280 Grade 1Cr18Ni9Ti GB/T 4232 Grade ML1Cr18Ni9Ti GB/T 4237 Grade 1Cr18Ni9Ti GB/T 4238 Grade 1Cr18Ni9Ti GB/T 4240 Grade 1Cr18Ni9Ti-Q GB/T 14975 Grade 1Cr18Ni9Ti GB/T 14976 Grade 1Cr18Ni9Ti GB/T 4240 Grade 1Cr18Ni9Ti-R GB/T 4240 Grade 1Cr18Ni9Ti-L GB 4239 Grade 1Cr18Ni9Ti GB 12770 Grade 1Cr18Ni9Ti GB 12771 Grade 1Cr18Ni9Ti GB 13296 Grade 1Cr18Ni9Ti GB 4356 Grade 1Cr18Ni9Ti GB 2270 Grade 1Cr18Ni9Ti SEW 470 Grade X12CrNiTi189 NF A35-578 Grade Z6CNT18-12 NF A35-580 Grade Z6CNT18-12B ISO 2604-2 Grade TS54~ EN 10095 Grade X8CrNiTi18-10 ASTM A403 Grade WP321 JIS G4307 Grade SUS321 JIS G4304 Grade SUS321 JIS G4309 Grade SUS321 JIS G4318 Grade SUS321 ISO 4955 Grade X7CrNiTi18-10
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 63.8449 — 73.9999
Cr 17.0 — 20.0
Ni 9.0 — 13.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
C 0.0 — 0.08
P 0.0 — 0.045
S 0.0 — 0.03

Properties

Mechanical

Tensile strength [ Rm ]

515.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Stainless Steel

The following suppliers might provide ASTM A403 Grade WP321:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM68038 to find materials similar to ASTM A403 Grade WP321.