Tensile strength Rm
515 MPa at 20 °C
Yield strength YS
205 MPa at 20 °C
Element
Weight %
Comment
62.74 - 74 %
17 - 20 %
9 - 13 %
0 - 0.1 %
0 - 0.03 %