Hardness, Brinell HB
0 - 341 [-] at 20 °C
Hardness, Rockwell C HRC
0 - 37 [-] at 20 °C
Element
Weight %
Comment
81.76 - 85.6 %
11 - 12.5 %
0.9 - 1.25 %
0.9 - 1.25 %
0.5 - 1 %
Processing history
nuts, washers
This material data has been provided by MetalInfo.