GB 3087 Grade 10

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Tensile strength Rm

0 - 475 MPa at 20 °C

Yield strength YS

195 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

98.17 - 99.41 %

Mn

0.35 - 0.65 %

Si

0.17 - 0.37 %

C

0.07 - 0.14 %

S

0 - 0.04 %

More

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.