GB 3531 Grade 09Mn2VDR

.XLSX
.PDF
Save

Description

Properties

Mechanical

Tensile strength Rm

430 - 570 MPa at 20 °C

Yield strength YS

0 - 290 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1.4 - 1.8 %

Si

0.15 - 0.5 %

V

0.02 - 0.06 %

S

0 - 0.03 %

P

0 - 0.03 %