GB/T 8162 Grade 12Cr1MoV

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Hardness, Brinell HB

179 [-] at 20 °C

Tensile strength Rm

490 MPa at 20 °C

Yield strength YS

245 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

96.56 - 98.05 %

Cr

0.9 - 1.2 %

Mn

0.4 - 0.7 %

Mo

0.25 - 0.35 %

C

0.17 - 0.23 %

More

This material data has been provided by MetalInfo.