GB 13788 Grade 60

Get more information
Contact Matmatch

Standards

Chemical composition

Element Weight %
Mn 0.5 — 0.8
C 0.57 — 0.65
Si 0.17 — 0.37
S 0.0 — 0.035
P 0.0 — 0.035