Customize your search with filters
Do you have any questions?
Hardness, Brinell HB
229 [-] at 20 °C
Element
Weight %
Comment
0.6 - 0.9 %
0.42 - 0.49 %
0.17 - 0.37 %
5E-4 - 3.5E-3 %
0 - 0.04 %
Processing history
quenched, tempered
This material data has been provided by MetalInfo.