Chemical composition

Element Weight %
Ni 1.3 — 1.8
Cr 0.8 — 1.1
Mn 0.5 — 0.8
C 0.42 — 0.49
Si 0.17 — 0.37
Mo 0.2 — 0.3
Cu 0.0 — 0.25
V 0.1 — 0.2
S 0.0 — 0.025
P 0.0 — 0.025