GB/T 3078 Grade 45MnB quenched, tempered

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Hardness, Brinell HB

229 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1.1 - 1.4 %

C

0.42 - 0.49 %

Si

0.17 - 0.37 %

B

5E-4 - 3.5E-3 %

S

0 - 0.04 %

More

Technological properties

Processing history

quenched, tempered

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.