Customize your search with filters
Hardness, Brinell HB
255 [-] at 20 °C
Reduction of area Z
30 % at 20 °C
Tensile strength Rm
655 MPa at 20 °C
Element
Weight %
Comment
0.5 - 0.8 %
0.47 - 0.55 %
0.17 - 0.37 %
0 - 0.04 %
0 - 0.04 %
Processing history
cold-dravn
This material data has been provided by MetalInfo.