Primary standard name

Properties

Mechanical

Tensile strength Rm

1470 - 1670 MPa at 20 °C

Yield strength YS

1100 - 1255 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.3 - 0.65 %

C

0.14 - 0.22 %

Si

0.12 - 0.3 %

Cr

0 - 0.3 %

Cu

0 - 0.3 %

More

Technological properties

Processing history

cold drawn

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.