GB 1499 Grade HRB400 deformed steel wire, rib

.XLSX
.PDF
Save

Description

Properties

Mechanical

Tensile strength Rm

0 - 1570 MPa at 20 °C

Yield strength YS

0 - 1340 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

S

0 - 0.04 %

Si

0 - 0.8 %

P

0 - 0.04 %

Mn

0 - 1.6 %

C

0 - 0.25 %

Technological properties

Processing history

deformed steel wire, rib