Reduction of area Z
45 % at 20 °C
Tensile strength Rm
530 MPa at 20 °C
Yield strength YS
315 MPa at 20 °C
Element
Weight %
Comment
0.5 - 0.8 %
0.32 - 0.4 %
0.17 - 0.37 %
0 - 0.04 %
0 - 0.04 %
This material data has been provided by MetalInfo.