GOST 1050 Grade 35 skinhard rolled product

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Reduction of area Z

35 % at 20 °C

Tensile strength Rm

590 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.5 - 0.8 %

C

0.32 - 0.4 %

Si

0.17 - 0.37 %

S

0 - 0.04 %

P

0 - 0.04 %

More

Technological properties

Processing history

skinhard

This material data has been provided by MetalInfo.