GOST 1050 Grade 35 quenched and tempered rolled product

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Tensile strength Rm

550 - 780 MPa at 20 °C

Yield strength YS

315 - 430 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.5 - 0.8 %

C

0.32 - 0.4 %

Si

0.17 - 0.37 %

S

0 - 0.04 %

P

0 - 0.04 %

More

Technological properties

Processing history

quenched and tempered

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Contact our suppliers

Select the region(s) and press “Contact suppliers“

China (5)
America (3)
Germany (6)
India (1)
Other regions