Reduction of area Z
35 % at 20 °C
Tensile strength Rm
610 MPa at 20 °C
Element
Weight %
Comment
0.5 - 0.8 %
0.37 - 0.45 %
0.17 - 0.37 %
0 - 0.04 %
0 - 0.04 %
Processing history
skinhard