GOST 1050 Grade 45 annealed or high-tempered hot-rolled and forged product

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Hardness, Brinell HB

197 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.5 - 0.8 %

C

0.42 - 0.5 %

Si

0.17 - 0.37 %

S

0 - 0.04 %

P

0 - 0.04 %

More

Technological properties

Processing history

annealed or high-tempered