GOST 5949 Grade 20_13_4_9

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Reduction of area Z

55 % at 20 °C

Tensile strength Rm

640 MPa at 20 °C

Yield strength YS

245 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

12 - 14 %

Mn

8 - 10 %

Ni

3.7 - 4.7 %

C

0.15 - 0.3 %

P

0 - 0.05 %

More

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Find a supplier

We can help you find a supplier of GOST 5949 Grade 20_13_4_9

We will evaluate your request and get back to you soon.