GOST 2060 Grade __62-1 drawn, 1/2 hard bar

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Hardness, Brinell HB

100 [-] at 20 °C

Tensile strength Rm

390 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

61 - 63 %

Sn

0.7 - 1.1 %

Sb

0 - 5E-3 %

Bi

0 - 2E-3 %

Fe

0 - 0.1 %

More

Technological properties

Processing history

drawn, 1/2 hard

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Find a supplier

We can help you find a supplier of GOST 2060 Grade __62-1 drawn, 1/2 hard bar

We will evaluate your request and get back to you soon.