EN 10225 Grade S355G9 normalized or normalized formed (+N)

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

The standard is applicable to steels for offshore structures, designed to operate in the offshore sector but not to steels supplied for the fabrication of subsea pipelines, risers, process equipment, process piping, and other utilities. It is primarily applicable to the North Sea Sector, but may also be applicable in other areas provided that due consideration is given to local conditions e.g. temperature.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

460 - 630 MPa

Show Material materials with Tensile strength of 460 - 630 MPa

Yield strength

20.0 °C

320 - 355 MPa

Show Material materials with Yield strength of 320 - 355 MPa

Chemical properties

PropertyValue

Aluminium

0.015 - 0.055 %

Show Material materials with Aluminium of 0.015 - 0.055 %

Antimony

0.01 %

Show Material materials with Antimony of 0.01 %

Arsenic

0.03 %

Show Material materials with Arsenic of 0.03 %

Bismuth

0.01 %

Show Material materials with Bismuth of 0.01 %

Boron

1E-3 %

Show Material materials with Boron of 1E-3 %

Calcium

5E-3 %

Show Material materials with Calcium of 5E-3 %

Carbon

0.12 %

Show Material materials with Carbon of 0.12 %

Chromium

0.2 %

Show Material materials with Chromium of 0.2 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Lead

0.01 %

Show Material materials with Lead of 0.01 %

Manganese

1.65 %

Show Material materials with Manganese of 1.65 %

Molybdenum

0.08 %

Show Material materials with Molybdenum of 0.08 %

Nickel

0.7 %

Show Material materials with Nickel of 0.7 %

Niobium

0.03 %

Show Material materials with Niobium of 0.03 %

Nitrogen

0.01 %

Show Material materials with Nitrogen of 0.01 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.15 - 0.55 %

Show Material materials with Silicon of 0.15 - 0.55 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

Tin

0.02 %

Show Material materials with Tin of 0.02 %

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

Vanadium

0.06 %

Show Material materials with Vanadium of 0.06 %