EN 12167 Grade CuCo2Be H055

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

Cuco2Be, mat. No CW104C, is counted among hardenable, low alloyed copper alloys. To the comparable make Cuco2Be, mat. No 2.1285, acc. to DIN 17666 : 1983-12 applies: CuCo2Be achieves compared to CuBe2 at slightly lower hardness and strength values higher electrical and thermal conductivity. The temperature for removal of workhardening approximates 500°C, high corrosion resistance. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: In relay and switch construction for high loadable, live springs and for radiant heaters at semi conductors. Furthermore for resistance and welding electrodes as well as for pistons, plunger and punching tools. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Wrought Copper High Copper Alloy

Hardness, Brinell

20.0 °C

55 [-]

Show Material materials with Hardness, Brinell of 55 [-]

Hardness, Vickers

20.0 °C

60 [-]

Show Material materials with Hardness, Vickers of 60 [-]

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper High Copper Alloy

Max service temperature, long

0 - 350 °C

Show Material materials with Max service temperature, long of 0 - 350 °C

Melting point

855 - 1090 °C

Show Material materials with Melting point of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Chemical properties

PropertyValue

Beryllium

0.4 - 0.7 %

Show Material materials with Beryllium of 0.4 - 0.7 %

Cobalt

2 - 2.8 %

Show Material materials with Cobalt of 2 - 2.8 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %