EN 1652 Grade CuSn6 M

Want to keep this datasheet? Save it now in your required format

Description

CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 - 8.82 g/cm³

Show Material materials with Density of 8.8 - 8.82 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

118 GPa

Show Material materials with Elastic modulus of 118 GPa

Elongation

20.0 °C

84 %

Show Material materials with Elongation of 84 %

250.0 °C

34 %

Show Material materials with Elongation of 34 %

350.0 °C

25 %

Show Material materials with Elongation of 25 %

500.0 °C

6 %

Show Material materials with Elongation of 6 %

Poisson's ratio

20.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Tensile strength

20.0 °C

345 MPa

Show Material materials with Tensile strength of 345 MPa

150.0 °C

350 MPa

Show Material materials with Tensile strength of 350 MPa

250.0 °C

295 MPa

Show Material materials with Tensile strength of 295 MPa

350.0 °C

210 MPa

Show Material materials with Tensile strength of 210 MPa

500.0 °C

145 MPa

Show Material materials with Tensile strength of 145 MPa

Unlock all property charts

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

200.0 °C

1.85E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.85E-5 1/K

650.0 °C

2.22E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.22E-5 1/K

800.0 °C

2.18E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.18E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 150 °C

Show Material materials with Max service temperature, long of 0 - 150 °C

Specific heat capacity

20.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Thermal conductivity

20.0 °C

75 W/(m·K)

Show Material materials with Thermal conductivity of 75 W/(m·K)

200.0 °C

98 W/(m·K)

Show Material materials with Thermal conductivity of 98 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

9.00E+6 S/m

Show Material materials with Electrical conductivity of 9.00E+6 S/m

200.0 °C

7.80E+6 S/m

Show Material materials with Electrical conductivity of 7.80E+6 S/m

Unlock all property charts

Electrical resistivity

20.0 °C

1.11E-7 Ω·m

Show Material materials with Electrical resistivity of 1.11E-7 Ω·m

200.0 °C

1.28E-7 Ω·m

Show Material materials with Electrical resistivity of 1.28E-7 Ω·m

Unlock all property charts

Specific Electrical conductivity

16 % IACS

Show Material materials with Specific Electrical conductivity of 16 % IACS

Chemical properties

PropertyValue

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Phosphorus

0.01 - 0.4 %

Show Material materials with Phosphorus of 0.01 - 0.4 %

Tin

5.5 - 7 %

Show Material materials with Tin of 5.5 - 7 %

Zinc

0.2 %