General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 8.8 - 8.82 g/cm³ Show Material materials with Density of 8.8 - 8.82 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 118 GPa Show Material materials with Elastic modulus of 118 GPa |
Elongation | 20.0 °C | 45 % Show Material materials with Elongation of 45 % |
Elongation A10 | 20.0 °C | 40 % Show Material materials with Elongation A10 of 40 % |
Elongation A100 | 20.0 °C | 35 % Show Material materials with Elongation A100 of 35 % |
Elongation A11.3 | 20.0 °C | 40 % Show Material materials with Elongation A11.3 of 40 % |
Poisson's ratio | 20.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] |
Tensile strength | 20.0 °C | 340 MPa Show Material materials with Tensile strength of 340 MPa |
Yield strength Rp0.2 | 20.0 °C | 230 - 270 MPa Show Material materials with Yield strength Rp0.2 of 230 - 270 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C Show Material materials with Max service temperature, long of 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) Show Material materials with Specific heat capacity of 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) Show Material materials with Thermal conductivity of 75 W/(m·K) |
200.0 °C | 98 W/(m·K) Show Material materials with Thermal conductivity of 98 W/(m·K) | |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m Show Material materials with Electrical conductivity of 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m Show Material materials with Electrical conductivity of 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m Show Material materials with Electrical resistivity of 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m Show Material materials with Electrical resistivity of 1.28E-7 Ω·m | |
Specific Electrical conductivity | 16 % IACS Show Material materials with Specific Electrical conductivity of 16 % IACS |
Chemical properties
Property | Value |
---|---|
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphorus | 0.01 - 0.4 % Show Material materials with Phosphorus of 0.01 - 0.4 % |
Tin | 5.5 - 7 % Show Material materials with Tin of 5.5 - 7 % |